Dengan memaksa gas buang melalui dinding antara saluran DPF, partikel disimpan di dinding, sehingga mengurangi jumlah polusi udara.
Ukuran | CPSI | Volume(L) | ||||
118*152.4 | 100/200 | 1.67 | ||||
118*254 | 100/200 | 2.78 | ||||
127*152.4 | 100/200 | 1.93 | ||||
127*180 | 100/200 | 2.3 | ||||
127*254 | 100/200 | 3.22 | ||||
144*152.4 | 100/200 | 2.49 | ||||
144*203 | 100/200 | 3.31 | ||||
144*254 | 100/200 | 4.44 | ||||
144*305 | 100/200 | 4.97 | ||||
190*152.4 | 100/200 | 4.32 | ||||
190*203 | 100/200 | 5.76 | ||||
190*305 | 100/200 | 8.65 | ||||
240*240 | 100/200 | 10.9 | ||||
240*305 | 100/200 | 13.8 | ||||
250*305 | 100/200 | 14.97 | ||||
267*267 | 100/200 | 14.22 | ||||
267*305 | 100/200 | 14,95 | ||||
286*305 | 100/200 | 17.07 | ||||
286*355 | 100/200 | 19.6 | ||||
305*305 | 100/200 | 22.8 | ||||
330*381 | 100/200 | 32.59 | ||||
Parameter | Satuan | Data | ||||
Bahan: Cordierite | berat% | 90 | 94 | |||
Koefisien Ekspansi Termal (20-800 ) | cm/cm/℃ | 1,8*10 | 1,5 × 10-6 | |||
Stabilitas Termal (20-650 ) | waktu | 1 | 3 | |||
Melunakkan Suhu | ℃ | 1420 | 1440 | |||
Kekuatan Kompresi | Memanjang | MPa | 16 | 16.9 | ||
Horisontal | MPa | 5 | 6.2 | |||
Berat Spesifik | Kg/L | 0,45-0,55 | 0,45-0,5 | |||
Porositas | % | 40-45 | 41 | |||
Tingkat penyerapan air | % | 23-25 | 23.8 |